Page number 1
Polymers DP-Susp. P/Lub. Polyester, Unsaturated - Soft and ductile 1596 Grinding Steps Surface Abrasive Lubricant Type Disc speed (rpm) Type Predosing/dosing Type Predosing/dosing Force (N) Holder direction Holder speed (rpm) Time (min) Polishing Steps Surface Abrasive Lubricant Type Disc speed (rpm) Type Predosing/dosing Type Predosing/dosing Force (N) Holder direction Holder speed (rpm) Time (min) PG SiC Foil #320 300 0/0 Water 0/0 20 >> 150 1 FG SiC Foil #500 300 0/0 Water 0/0 20 >> 150 1 FG 2 SiC Foil #1200 300 0/0 Water 0/0 20 >> 150 1 FG 3 SiC Foil #4000 300 0/0 Water 0/0 20 >> 150 1 DP MD-Mol 150 DP-Susp. P 3 µm 3/6 DP-Red 3/12 30 >> 150 4 DP 2 MD-Nap 150 DP-Susp. P 1 µm 3/6 DP-Blue 3/14 20 >> 150 3 OP MD-Chem 150 OP-S, 0.25 µm 1/10 10 >< 150 1 Method comments The method is developed to fit a standard equipment configuration with 30 mm specimen on 300mm disc. Dosing levels are valid for following equipment: Tegramin, AbraPol and LaboPol For advice on how to adjust the method to fit your equipment, please take a look at Preparation Parameters. The preparation time for the plane grinding (PG) step depends very much on the condition of the samples and if they are prepared as single specimens or clamped in a specimen holder. Please check the samples after the first step and repeat it if necessary. Take a look at Preparation Parameters